Step 1


Step 1
A multi-turn ring of PRO One flux-cored wire is placed on the outside diameter of the tube. The proper volume of filler metal has been calculated and formed into a preformed ring that will produce a strong, hermetic joint.

Step 2 - Flux dissolves and absorbs oxides that form during heating and facilitates successful brazing.


Step 2
During the initial phase of heating, brazing flux escapes from the preformed ring, distributing flux throughout the joint area. When active, the flux is drawn by capillary attraction down into the joint.

Step 3 - Flux protects the filler metal and material surface as the filler metal is drawn down into the joint.


Step 3
The flux is now active and the filler metal begins to melt. The alloy, when fully molten, will follow the flux (and capillary attraction) into the joint. The minimal amount of flux in the cored wire reduces flux inclusions and produces high-strength joints.

Step 4


Step 4
PRO One produces sound braze joints with complete alloy penetration and a uniform fillet that is visible at the surface.
Contact Us Today!
Please contact Protechno for more information or to talk to a Technical Representative about the PRO One product that's right for you.

To find out more about Protechno SA. go to www.protechnogasflux.com
Protechno SA.
ZAE Les Chaumes - BP27
24600 RIBERAC - FRANCE
protechno@protechnogasflux.com
(33) 05 53 92 53 00 phone
(33) 05 53 92 53 18 fax
PROTECHNO S.A. - ZAE Les Chaumes - BP27 - 24600 RIBERAC - FRANCE
http://www.protechnogasflux.com | mailto:protechno@protechnogasflux.com
phone (33) 05 53 92 53 00 | fax (33) 05 53 92 53 18

Copyright © 2003 PROTECHNO SA.
All rights reserved.